exterior walls

Horizontal surfaces like awnings, chajjas, terrace borders, etc. should be given one additional coat for better protection as these areas are prone to water accumulation.

No interior primer, putty or plaster of paris should be applied under the exterior finishes. Doing so will affect the performance of the paint.

Sr. No.

Name of Paint

Thinner for 1 ltr/kg of paint in mls

Thinner

No. of coats recommended and application

Undercoat applied

Recoating Time (hrs)

 

 Primer

 

 

 

 

 

1

AP Seal - WB

1-2 ltrs water in 20 ltr pack

Water

2 Coats - Brushing/Roller

 

4-5 hrs

2

AP Seal - SB

400 - 800 ml Turpentine in 4 ltr pack

Turpentine

2 Coats - Brushing/Roller

 

4-5 hrs

3

Asian Paints Exterior Wall Filler

7 - 8 ltrs water in 20 ltr pack

Water

1 Coats - Brushing/Roller

 

4-6 hrs

4

Asian Paints Exterior Sealer

1.6 ltrs water in 4 ltr pack

Water

1 Coats - Brushing/Roller

 

4-6 hrs

5

Asian Paints Crack Bridging Wall Primer

0.5 - 1 ltr water in 10 ltr pack

Water

2 Coats - Brushing/Roller

 

4-5 hrs

6

Asian Paints Exterior Wall Putty

7 - 8 ltrs water in 20kg pack

Water

1-2 Coats as required-Putty Knife

 

6-8 hrs

 

Top Coat

 

 

 

 

 

1

Apex Ultima Exterior Emulsion

4 - 5 ltrs water in 20 ltr pack

Water

2 Coats - Brushing/Roller

Exterior Wall Filler/AP Seal WB/Crack Bridging Wall Primer If Required

4-6 hrs

2

Apex Weather Proof Exterior Emulsion

8 ltrs water in 20 ltr pack

Water

2 Coats - Brushing/Roller

Exterior Wall Filler/AP Seal WB/Crack Bridging Wall Primer If Required

4 hrs

3

Apcolite Ace Exterior Emulsion

4 - 6 ltrs water in 20 ltr pack

Water

2 Coats - Brushing/Roller (1st Coat-25-30%,2nd Coat-15-20%) For Repainting 30% with Water)

Exterior Wall Filler/AP Seal WB/Crack Bridging Wall Primer If Required

4-6 hrs

4

Ace Exterior Emulsion

4 - 6 ltrs water in 20 ltr pack

Water

2 Coats - Brushing/Roller (1st Coat-25-30%,2nd Coat-15-20%)

Exterior Wall Filler/AP Seal WB/Crack Bridging Wall Primer If Required

4 hrs

 

*New surfaces must be coated with one additional coat of self-priming with water (1:1 by volume).

Image